more glass and metal coated

last night with the radio keeping me company
i heated emulsion and scrubbed glass and
coated 6- 5×7, 4- 4×5 glass plates  1 – 4×5 metal sheet, and 2 trimmed small ones for 35mm and MF.
they chilled and now are drying out in the dark ..

i hate waiting and wish SGE would dry out quicker, but it doesn’t …

 

This entry was posted in alternative process photography, film development technique, images on glass and metal, liquid emulsion, photographs and tagged , , , , , , , , , , , , .